ProgHouseDJ
Member For 1 Year
hello!
I have been using thick stainless round wire for a while with no problems, and stainless cores with kanthal wrapping for Claptons. I got some 36g stainless to make all stainless Claptons, with 28 and 26 cores. After building for a couple different RDAs and RTAs, I’m noticing a fairly strong metallic flavor. Is this an indication of something going wrong, does it go away with time, and is there a way to prevent it from happening?
Thanks!
I have been using thick stainless round wire for a while with no problems, and stainless cores with kanthal wrapping for Claptons. I got some 36g stainless to make all stainless Claptons, with 28 and 26 cores. After building for a couple different RDAs and RTAs, I’m noticing a fairly strong metallic flavor. Is this an indication of something going wrong, does it go away with time, and is there a way to prevent it from happening?
Thanks!